Above 600 °C, creep resistance and microstructural stability decide service life. ROBAN supplies the certified alloys that turbine OEMs and furnace builders specify by grade.
UNS N06002, DIN W. Nr. 2.4665
8.23 g/cm3 · 1260-1355℃
UNS N06635
8.75 g/cm3 · 1335-1380℃
UNS R30188
8.98 g/cm3 · 1315-1410℃
UNS N06230, DIN W. Nr. 2.4733
8.97 g/cm3 · 1301-1371℃
UNS R30556
8.23 g/cm3 · 1330-1415℃
UNS N06625, DIN W. Nr. 2.4856
8.44 g/cm3 · 1290-1350℃
UNS N07718, DIN W. Nr. 2.4668
8.23 g/cm3 · 1260-1335℃
UNS N07750, DIN W. Nr. 2.4669
8.28 g/cm3 · 1393-1427℃
UNS N08810, DIN W. Nr. 1.4958
7.94 g/cm3 · 1357-1385℃
UNS N08811, DIN W. Nr. 1.4959
7.94 g/cm3 · 1357-1385℃
UNS S66286, DIN W. Nr. 1.4980
7.94 g/cm3 · 1370-1430℃
UNS N08926, DIN W. Nr. 1.4529
8.1 g/cm3 · 1320-1390℃
All grades in this line are available in the following forms. Custom sizes, tolerances and cut parts are produced to your drawing.
EN 10204 3.1 material certificate with every order, issued against the actual heat analysis.
Heat number traceability from cast or billet through forming, machining and final inspection.
Dimensional, ultrasonic, eddy current, PMI and hardness testing to your drawing and the applicable standard.
Send grade, form, dimensions, quantity and application. You receive a specification check, a price and a lead time — not a catalogue reprint.
Request a Quote